Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels. Designation: A 262-01
Enregistré dans:
| Format: | Livre |
|---|---|
| Langue: | anglais |
| Publié: |
ASTM,
2001
|
| Sujets: | |
| Tags: |
Pas de tags, Soyez le premier à ajouter un tag!
|
Documents similaires: Standard Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels. Designation: A 262-01
- Effect of precipitation on the pitting corrosion of high nitrogen austenitic stainless steel P560 : Diplomová práca
- Vplyv plastickej deformácie na koróznu odolnosť austenitických nehrdzavejúcich ocelí = Influence of plastic deformation on the corrosion resistance of austenitic stainless steels : Dizertačná práca
- Temperature dependent evolution of secondary phases in Cr-Mn-N austenitic steel
- Materiálová analýza tenkostenných rúrok z austenitickej nehdrdzavejúcej ocele AISI 304L = Material analyse light pipes from austenitic stainless steel AISI 304L : Bakalárska práca
- Vplyv časovo-teplotných expozícií na koróznu odolnosť vo vybraných austenitických nehrdzavejúcich oceliach = Influence of time-temperature exposures on corrosion resistance of specified types of austenitic stainless steel : Bakalárska práca
- Materiálová analýza tenkostenných rúrok z austenitickej nehrdzavejúcej ocele = Material analysis of thin-walled pipes made from austenitic stainless steel : Bakalárska práca